Практические результаты создания стеклометаллокомпозитного стержня

Гридасова Екатерина Александровна, Любимова Ольга Николаевна · CyberLeninK (CyberLeninka) · 2012

Glass has a high compressive strength and low impact strength. The strength of glass in compression is a lot higher than the strength of glass in tension, and it varies within the range of 500-1,250 MPa. Whenever the glass is in compression, it can compete with the properties of metal in terms of its strength. The tensile strength of glass under tension is 30-50 MPa. The reason for that is the fact that the strength of glass is strongly dependent on the state of its surface. Methods of increasing the strength of glass have been the subject of research projects implemented at Far Eastern Federal University. The objective is to apply compressive stresses that would prevent any defects in the surface layer and harden the surface to improve the glass resistance to mechanical stresses and isolate it from the environment. Creation of a composite rod made of glass grade C49-1 (3С5Na) and steel E235C (ISO standard) manufactured through the employment of diffusion bonding represents a practical result of the research. Its analysis has proven the presence of full contact, absence of cracks and poor penetration alongside the welding zone. Microscopy methods of analysis have demonstrated the presence of the transition zone in the points of interface of materials. The results of the spectral analysis prove the penetration of Fe-cations into the glass down to the depth of 30 microns. The chemical analysis of the zone of diffusion proves that the crystalline structure, or fayalite (Fe2SiO4), is formed in the glass. The rod strength analysis has demonstrated its high compressive

Cited by 0 works.

Authors