Эффективность применения наполнителей при производстве фанеры на малотоксичных карбамидоформальдегидных смолах
Мурзин Виктор Сергеевич, Кантиева Екатерина Валентиновна, Пономаренко Лариса Викторовна · CyberLeninK (CyberLeninka) · 2012
The increase in production output for export meeting the requirements of European standard for the class of emission of formaldehyde from these products led to the need for the production and use of so-called low-toxic resins containing free formaldehyde not more than 0.15 %. Use of low-toxic resins allowed producing products corresponding formaldehyde emission class E1 and E2. In particular, the content of formaldehyde per 100 g of absolutely dry mass of plywood of E1 grade is up to 10 mg inclusive, for E2 more than 10 mg to 30 mg inclusive. Synthesis of low-emission UFR is conducted at a molar ratio of urea to formaldehyde of 1:1 to 1:1.2, which inevitably leads to decrease in their adhesive properties, changes in the mechanism of hardening at hot bonding (WPB production, plywood), except that they are synthesized at a lower final viscosity. In the manufacture of plywood, especially from birch veneer, the viscosity of the adhesive should be much higher considering the high permeability of the birch wood. The low viscosity of UFR can cause excessive penetration into the permeable timber veneer at plywood pressing and formation of hungry glue joint, which leads to decrease in bond strength. In the present work refinement formulation of adhesives in particular number of fillers for use in the manufacture of plywood of modern brands of low-toxic resins was carried out. The tests were carried out with such fillers as wood flour, rye flour, kaolin. The data on the optimal number of organic (wood flour) and mineral (kaolin) fillers for adhesive based on centrally produced resin KF-MT-15 suggests the possibility of its widespread use for the production of plywood and furniture.
Cited by 0 works.