Практическое определение допуска к эксплуатации элементов сварного соединения магистрального газопровода

Буклешев Дмитрий Олегович · Universum · 2016

Operating practice of the gas-main pipeline shows that the main factors causing destruction are the defects such as hot-spot corrosion, cracks by the corrosion cracking under the strain and deformation in the joint mounting as well. It is established, that at the gas-main pipeline welded connections and weld-affected zone segments of the annular coupling, made by manual arc fluid welding, under the influence of constructive, technological and assembly factors there can be zones with abnormally high operational stress concentration. Additional impact on the weld-affected zone by the residual welding stress and internal operational stress reduces the resistance of welded joint to fragile mechanical destruction and corrosion cracking under the strain, and that determines the increased requirements to diagnostic works. Stress concentration in the weld-affected zones of welded joints occurring due to thermal stresses causes metal inhomogeneity and defects emergence. In the article functioning methods on the operational feasibility definition of the gas-main pipelines welded joints and weld-affected zones by the criterion of the existed defects are analyzed. Practical application of two nondestructive control methods, carried out for definition of the defect character and existence in the welded connections, is considered. As a subject of a control the defective welded connection of the gas-main pipeline which isn't permitted to operation is used. The first method represents radiographic research of a control subject and is the most widespread control method of welded connections at the moment. The other control method is based on metal magnetic memory. Metal magnetic memory method allows to do dislocations and defects assessment, both in the main body, and in local zones of the pipeline stress concentration.

Cited by 0 works.

Authors