Исследование процесса обесшламливания низкосортных сильвинитовых руд Тюбегатанского месторождения

Самадий Муроджон Абдусалимзода, Бобокулов Акбар Носирович, Росилов Мансур Сиргиевич et al. · Universum · 2016

Results of researches of process deslurrying of low-grade sylvinite ores of the Tyubegatan deposit with the contents of 23,2-30,7 % KCI and 3,25-4,95 % of the insoluble rest in water a two-phasic hydromechanical method in hydrocyclones and with additional installation of a hydroseparator at the third stage are resulted. It is noticed, that insoluble impurity in water of sylvinite ores of the Tyubegatan deposit are presented, basically, lightly slurring carbonates (magnesite, dolomite) and sulphatic (anhydrite, bassanite) minerals on 65 ÷ 70 % from the general quantity of i.r. in ore. Investigated process deslurrying of sylvinite ores with the low 28,0-30,0% contents of potassium chloride and the contents i.r. no more than 3,2%, production schedules corresponding to requirements, under the two-phasic scheme it is established, that sand of I stage of a hydrocyclone contain 1,79-1,88 % i.r. after the second hydrocyclone sand contain from 2,38 to 2,82 % i.r. On a feed sylvinite flotation arrive sand with the content of 29,5-31,1 % KCI and 1,94-2,06 % i.r. At giving of incorporated sand after 1 and 2 stages of deslurrying in hydrocyclones on the third stage in a hydroseparator technological indicators of process of deslurrying improve. Sand after the third stage of deslurrying or a feed the basic sylvinite flotation contains 29,8-31,7 % KCI and 1,36-1,42 % i.r., that corresponds to the parameters specified in production schedules. Degree of deslurrying raises to 16,3-17,2 %. Researches with sylvinite ore containing 20,10-30,25 % KCI and 3,25-5,30 i.r. have shown, that potassium chloride decrease in initial ore leads to sharp decrease KCI in sand of 1 both 2 stages of deslurrying and to increase i.r. to 1,87-2,91 % and 2,49-5,13%, accordingly. Installation of an additional third stage of deslurrying with hydroseparator application gives the chance to lower i.r. to the demanded contents in a feed sylvionite flotation. The content i.r. makes 1,43-2,01 % at content KCI of 23,4-32,0 %.

Cited by 0 works.

Authors