Shiomi Kikuchi, Kunikazu Tomita, 義郎 元山 et al. · Journal of Japan Institute of Light Metals · 1980
Stress relaxation tests were carried out in the region of steady state deformation at temperatures 623, 673 and 723K. The stress relaxation rate is proportional to the stress in the short period from beginning of the relaxation and subsequently to third power of the stress. The internal stress and the mobile dislocation density can be estimated on the basis of stress relaxation curves in the region in which the stress relaxation rate is proportional to the stress. The internal stress obtained in the relaxation test is in accordance with that in the dip test. The mobile dislocation density depends on the steady state stress and is expressed as: ρmα(σs/μ)2
Cited by 7 works. doi:10.2464/jilm.30.480 Open-access PDF