급속응고 고망간 강판의 탄화물 석출에 미치는 첨가원소의 영향

김형수, 최창범, JinYeong Bak et al. · 대한금속재료학회지 · 1990

When the rapidly solidified standard high Mn steel strips were reheated, the precipitation curve of carbide was likely a C-curve which had the nose at about 600-700℃. The precipitation curve of pearlitic constituents(PC) was also likely a C-curve having the nose at about 600℃. By addition of alloying elements(Cr, V), the temperature ranges of the carbide and PC precipitation were enlarged and the time of their precipitation was earlier. The quantities of the carbide and PC precipitation were increased and were observed much more in the V-added specimen. Regardless of the alloying elements(Cr, V), carbide was formed in the shape of film at the grain boundaries at 500-700℃. With the increase of heating time, the shape of carbide film was grown like plate and subsequently PC nucleus was formed at the plate-like precipitations and grown. The hardness of the (Cr, V) added specimen was higher than that of the standard specimen. The increased hardness was mainly affected by PC rather than carbide. V has more accelerated the formation of carbide and PC than Cr.

Cited by 0 works.

Authors