Исследование перколяционного выщелачивания ценных компонентов из хвостов обогащения Дашкесанского горно-обогатительного комбината
А. А. Гейдаров, Ch.M. Kashkai, A. A. Gulieva et al. · CyberLeninK (CyberLeninka) · 2016
The research has been carried out on samples of current waste enrichment factory of Dashkesan mining and processing plant (Azerbaijan) containing Al, Ca, Fe, Si, Co, Cu, Zn, Mn. Main phase waste enrichment phases are quartz, kaolinite, clinochlore, calcite, dolomite, pyrite, hematite, andradite. As for exsisting technologies, the simplest and cheapest method to reprocess raw matyerial of this type are heap and underground leaching. Rational parameters and regimes of leaching process for laboratory purposes have been determined. Principal potentials for extraction Al, Co, Cu, Zn, Mn through the use of sulphuric acid solutions extraction out of current wastes in heap leaching mode have been defined. It revealed that following the sixth cycle of irrigation with 1n sulfuric acid there has been extracted 65,9% Co, 30,5% Cu, 25,1% Zn, 17,5% Mn, 4,1% Fe, 1,82% Al.
Cited by 0 works.