РАЗРАБОТКА МЕТОДА ОЦЕНКИ ОСТАТОЧНОГО РЕСУРСА МАГИСТРАЛЬНЫХ ГАЗОПРОВОДОВ, ИМЕЮЩИХ ДЕФЕКТЫ КОРРОЗИОННОГО ПРОИСХОЖДЕНИЯ

O.A. Nasibullina, Алексей Габдуллович Гареев · 2016

One of the most hazardous types of the gas pipeline rupture is a stress-crack corrosion (SCC) of external cathodically -protected surface .SCC appears in the form of multiple or single cracks on the metal surface. And therefore a problem of the further gas pipeline’s operation with such defects is arose. In this work the main methods of the gas pipeline residual life estimation have been considered. At calculation of the steel structure service life , subjected to general pit corrosion and to SCC, mainly two methods are used : calculation of “boiler “ formula is made or semiempirical model of the Battelle Institute is used. For researching the justice of the semiempirical model of the Battellte Institute computer calculations were made in this work, that allows to determine the critical crack length for tubes 1420 mm in diameter and with wall thickness 14 - 20 mm. The results of the computerized modeling showed that using the given dependence for cracks with depth less then 3-4 mm isn’t correct . In connection with this the calculation of the critical crack length for tubes 1420 mm in diameter with cracks at depth 5 - 16 mm and with wall thickness15 - 20 mm were made . It was shown that knowing of the crack depth or “slit -shaped defect, one can define it’s permissible length . And also the calculation of a hazard rate of the discovered defects have been carried in this work. Computer program allowing to determine the rated pressure on the tube sections having extended as well as small centers of corrosion have been formed .

Cited by 0 works.

Authors