ПОВЫШЕНИЕ БЕЗОПАСНОСТИ ЭКСПЛУАТАЦИИ ТРУБОПРОВОДОВ, ПОДВЕРЖЕННЫХ КОРРОЗИОННОМУ РАСТРЕСКИВАНИЮ

О. А. Гареева, Марат Замирович Ямилев, Александр Васильевич Лягов et al. · 2011

Stress corrosion cracking appears due to single and multiple cracks emerging on the outer surface of the pipe. All existing techniques of retests of the main gas pipelines are based on the assumption of presence only single cracks. Therefore the question on applicability of these actions for the centers with plural cracks is opened now. We performed a study of the focal zone is destroyed a gas pipeline, which has multiple cracks. Based on these results it is shown that the most dangerous are the deepest cracks. The methods applied at test of the main gas pipelines, can be used and for the pipes, having plural cracks.