간헐 압축응력완하 시헙법을 이용한 불소 실리콘 오링의 수명 예측 연구
이진혁, 배종우, 윤유미 et al. · 한국추진공학회 학술대회논문집 · 2016
Intermittent CSR testing was used to investigate the degradation of a FVMQ O-ring, and also the prediction of its life-time. An intermittent CSR jig was designed taking into consideration the O-ring’s environment under use. Degradation of O-rings by thermal aging was observed between 60℃ and 170℃. O-rings showed non-linear degradation behavior under 100℃. At 50% of failure condition, predicted life-times were 32.6 years by Arrhenius plot and 26.2 years by WLF plot.
Cited by 0 works.