극한지 가스배관의 파괴인성 평가에 관한 연구
김익중, 김우식, 박준식 et al. · 대한기계학회 춘추학술대회 · 2016
Recently, increasing the gas pipeline construction in permafrost area (air temperature is lower than -40℃). So, The line-pipe steel has sufficient energy absorption capacity (toughness) to arrest a running fracture to brittle fracture. This involves ensuring the pipe material toughness is sufficient to arrest a running brittle fracture. Brittle fracture propagations with one of the first challenges to gas pipelines integrity. Brittle fractures of 15 to 60 km occurred from late 1930s to mid 1960s. PRCI was founded to solve this problem through AGA/NG-18 program. Brittle fracture phenomena were identified as experimental observations based on the results of West Jefferson vessel burst test at PRCI in 1961. As a result, Pressed-notch(PN) DWTT developed in this program, and there is a presented as a brittle fracture evaluation most of the current line-pipe design codes(ASME B31.8, CSA, DNV, etc.,). Of course, simple cheap test as alternative to charpy test. However, Original DWTT was developed on pre-1970 steels that have less than 50ft-lb of charpy upper-shelf energy. In mid 1970s first noticed PN-DWTT didnt work to predict transient temperature in burst test on much high grade line-pipe steel (CVN=220ft-lb). Since then, the issue of the fracture toughness evaluation of high grade line-pipe steel is constantly being raised. In this paper, evaluation of high grade line-pipe steel in permafrost area gas pipelines of API 5L X65 and X70 using Charpy V-notch (CVN) test and PN-DWTT. Consequently, compared to between CVN and PN-DWTT results to determined the correlation, and to establish the fracture toughness evaluation of high grade line-pipe steel.
Cited by 0 works.