실란 커플링제가 무용제형 에폭시계 주차장용 콘크리트 표면 마감재의 물리적 성능에 미치는 영향
채우병, 성동연, 서상교 · 대한건축학회 학술발표대회 논문집 · 2012
This study attempted to the effect on the physical performance of silane coupling agent on solventless epoxy-based concrete surface finishing material for parking floor. Tests were carried out in accordance with KS F 4041 and KS F 4937. The results of compressive strength, flexural compressive are 95.6N/㎟, 25.4N/㎟ and after wheel moving load testing, average abrasive depth is 0.96mm, these results satisfied the quality standard of KS F 4041, KS F 4937. As conclusion, this study confirmed that the silane coupling agent greatly effected on the physical performance of solventless epoxy resin.
Cited by 0 works.