Підвищення тріщиностійкості при високошвидкісному наплавленні на низькій погонній енергії валків
Сергій Вікторович Щетинін, Віра Щетиніна, A. V. Koval et al. · The Scientific Issues of Ternopil Volodymyr Hnatiuk National Pedagogical University Series pedagogy · 2018
The rolling-mill rolls crack resistance increases at high-speed surfacing with low heat input. The rolling-mill rolls operate under high specific pressures conditions and are produced of high-carbon steel, prone to cracking formation. Therefore crack resistance increase is an important scientific and technical problem. The effective way to improve crack resistance is high-speed electric arc surfacing with low heat input, which changes the arc existence conditions, decreases heat input, increases the rate of the liquid metal heating and cooling. This results in a change in the bath crystallization conditions and the deposited metal quality. The welding speed increase leads to column cooling and the pinch-effect intensification, arc diameter reduction and the heat input concentration, which makes it possible to increase the process speed. Increasing crack resistance mechanism at high-speed surfacing with low heat input, the influence of welding speed regularities on the processes in the weld pool, the weld formation, deformation, welding stresses and the weld metal crack resistance has been established. With the surfacing speed increase both the heat input and heat input rate, and deformation and welding stresses decrease, which provides crack resistance increase.With the welding speed increase the liquid metal crystallization rate increases proportionally, the crystals do not have time to grow, which ensures the microstructure grinding, the interatomic bond forces increase, the tensile strength increase, and increasing crack resistance. Concurrent welding stresses decrease and the tensile strength increase at high-speed surfacing with low heat input provide for increasing crack resistance of rolling-mill rolls. The high-speed surfacing with low heat input which provides welding stresses decrease and microstructure reduction, cracking prevention of rolling-mill rolls and wear resistances increase has been developed
Cited by 0 works. doi:10.31498/2225-6733.37.2018.160249