Влияние водорода на характер разрушения трубопроводов

Марат Фаритович Сунагатов, Павел Викторович Климов, Айдар Кабирович Гумеров · НАУЧНО-ТЕХНИЧЕСКИЙ ЖУРНАЛ «ПРОБЛЕМЫ СБОРА, ПОДГОТОВКИ И ТРАНСПОРТА НЕФТИ И НЕФТЕПРОДУКТОВ» · 2010

Background The so-called stress-corrosion cracking on the gas pipelines is widely known, it is responsible for more than a half of occurring accidents. Aims and Objectives To analyze the mechanism of hydrogenation and cracking of metal pipes during operation; to propose the ways of destruction slowdown. Methods The laboratory studies of steels with a tensile strength from 300 to 800 MPa were conducted. Results 1. The intensity of embrittlement and cracking of the pipeline depends on the intensity of the atomic hydrogen source and on the stress state of the pipeline. 2. It is necessary to exclude the atomic hydrogen sources from the metal pipes surface for pipeline stress-corrosion cracking slowdown, wherefore the insulation coating should be restored. 3. Electrochemical protection of pipelines cannot prevent stress-corrosion cracking by the hydrogenation mechanism.

Cited by 0 works. doi:10.17122/ntj-oil-2010-3-35-42

Authors