ИССЛЕДОВАНИЕ ФАКТОРОВ, ВЛИЯЮЩИХ НА ЭРОЗИОННЫЙ ИЗНОС ОБОРУДОВАНИЯ УСТАНОВОК ДЕГИДРИРОВАНИЯ В КИПЯЩЕМ СЛОЕ МИКРОСФЕРИЧЕСКИХ АЛЮМОХРОМОВЫХ КАТАЛИЗАТОРОВ В УСЛОВИЯХ ПРОМЫШЛЕННОЙ ЭКСПЛУАТАЦИИ
А. Н. Катаев, Alexander A. Lamberov, Svetlana R. Egorova et al. · Катализ в промышленности · 2014
Main problems related to the operation of high strength impregnated microspherical aluminochromium catalysts in the process of dehydrogenation of isoparaffins are discussed. A focus is made on the problem of erosive wear of the walls of overflow pipelines during operation of the mixture of the impregnated isobutane dehydrogenation catalyst (IDC) with the traditional IM-2201C catalyst and on the ways to resolve the problem. It is established that the main reason for intensifying the erosive wear is the rise of the catalyst particle pulse due to an increase in the average particle size and an increase in the transport gas flow rate: Upon substitution of the mixture of IM-2201C and IDC (70:30) for IM-2201C, the average particle size of the equilibrium catalyst increases from 68 to 74 μm. The optimal fraction composition of the high-strength catalytic system is calculated to provide no increase in the abrasion activity but a decrease in the feeding rate of the transport gas and preservation of the 20–30 wt.% proportion of particles of 20–40 μm in size. It is recommended to manufacture a commercial batch of the highstrength catalyst with the optimal fraction composition in order to use it without addition of IM-2201C for the industrial isobutane production.
Cited by 0 works.