Определение концентрации свободных носителей заряда в легированных бором кремниевых нанонитях при помощи инфракрасной спектроскопии в режиме нарушенного полного внутреннего отражения

E. A. Lipkova, А.И. Ефимова, К.А. Гончар et al. · Физика и техника полупроводников · 2019

Attenuated total reflection infrared spectroscopy was used to determine the free charge carrier concentration in the arrays of silicon nanowires of characteristic transverse dimension of 50–100 nm and the length of the order of 10 μm which were formed on low-doped crystalline p-type silicon via metal-stimulated chemical etching and subjected to additional thermodiffusion boron doping at the temperatures 850–1000 оС. It was found out that the free hole concentration varies from 5•1018 to 3•1019 cm-3 depending on the annealing temperature and reaches it’s maximum at 900–950 оС. The results can be used to expand the scope of silicon nanowires application in photonics, sensorics and thermoelectric power converters.

Cited by 0 works. doi:10.21883/ftp.2019.11.48455.9157 Open-access PDF

Authors