한중콘크리트의 관리재령 연장을 이용한 설계기준강도 확보 기법
이영준, 이혁주, 한준희 et al. · 한국건축시공학회 학술.기술논문발표회 논문집 · 2018
The purpose of the research is suggesting the temperature compensation strength for Unicode of constructure standard from Ministry of land, infrastructure and transport. As a result, for the concrete mixture with 100 % OPC, 6, and 3 MPa of compensating strength values were necessary when the temperature were from 4 to 9 ℃, and from 9 to 17°C, respectively. Additionally, when the temperature was higher than 17℃, compensating strength value was not necessary. In the case of 20 % of blast furnace slag replaced concrete mixture, 9, 6, and 3 MPa of compensating strength values were necessary when the temperature were from 4 to 6℃, from 6 to 12℃, and higher than 17℃, respectively.
Cited by 0 works.