고강도 탄소강 FCA 용착금속의 고온균열 저항성과 저온 충격인성에 미치는 보론과 망간의 영향
박수길, 조영호, 지춘호 et al. · 대한금속재료학회지 · 2019
The hot crack resistance and mechanical properties of flux cored arc (FCA) welds were investigated with three kinds of welding consumables having different boron (B) and manganese (Mn) contents for high strength carbon steel. The hot crack resistance, measured from self-restraint testing, strongly depended on the amount of B in the welding consumable. Welding consumables with higher B contents resulted in longer total crack length and an increased number of cracks. Boron was intensely detected near the grain boundary of the weld centerline by secondary ion mass spectrometry (SIMS) analysis, and precipitated with boron carbide (Fe23(C,B)6), as analyzed by transmission electron microscopy (TEM). This promoted hot crack propagation in the high strength carbon steel welds. However, removing B from the welding consumable decreased the low temperature toughness for root and face weld metals, due to the growth of ferrite side plate (FSP), compared with welding consumables having more B or Mn contents. The addition of Mn in the weld metal suppressed the formation of FSP and increased low temperature toughness. Therefore, the minimization of B and the supplement of Mn successfully achieved hot crack resistance and low temperature toughness for high strength carbon steel welds of 550 MPa tensile strength. (Received October 5, 2018 ; Accepted November 17, 2018)
Cited by 0 works.