ОЦЕНКА РАБОТОСПОСОБНОСТИ ТРУБ, ИМЕЮЩИХ ДЕФЕКТЫ КОРРОЗИОННОГО ПРОИСХОЖДЕНИЯ

Алексей Габдуллович Гареев, O.A. Nasibullina, Ildus G. Ibragimov · НАУЧНО-ТЕХНИЧЕСКИЙ ЖУРНАЛ «ПРОБЛЕМЫ СБОРА, ПОДГОТОВКИ И ТРАНСПОРТА НЕФТИ И НЕФТЕПРОДУКТОВ» · 2016

Background Underground corrosion of pipelines often occurs in the form of pits. Pit geometrical parameters are determined by flaw detection methods, intra-pipe flaw detection for underground pipelines, in particular. Various devices are used for visually detected pits. Metal loss in the case of pitting is determined using plasticine replica. Durability of shell designs, including pipes subject to pit corrosion, is calculated on the basis of ANSI/ASMEB31G technique. It is based on a series of tests of the full-length pipes with the natural and artificially caused defects, carried out at Battel’s Institute (USA) and resulted in empirical dependences. Aims and Objectives Determine the critical length of a crack for1420-mm pipes with wall thickness of 15 - 20 mm. Depending on the pit geometrical dimensions, carry out calculations in rectangular or parabolic approximation. Apply parabolic approximation to deep and short-length pits. Use rectangular approximation with respect to shallow and lengthy pits. Methods Pit geometrical parameters were determined by flaw detection methods. Metal loss in the case of pitting is determined using plasticine replica. For this purpose, a plasticine layer was pressed into the oiled metal surface. Plasticine remainder was removed cleaned up by a flexible metal ruler. The volume of corroded metal was determined by a measuring cylinder. The mass of the lost metal was found by multiplying the received volume by metal density. Durability of shell designs, including pipes subject to pit corrosion, is calculated on the basis of ANSI/ASMEB31G technique. Conclusion The carried-out analysis of corrosion defect of pipelines revealed the regularity that, knowing depth of a pit or equivalent crack-like defect, it is possible to determine its maximum admissible length which does not result in the changed form (opening) of the pipe. Regardless of the length of corrosion defect, pipes with pit depth of 0,8δ and more are subject to replacement; here δ is the pipe wall thickness. Where the depth of pits is less than 0,2δ, the pits are considered harmless, and the construction can be operated without limitations. I.e., calculations are carried out where the depth of pits is within the range (0,2 - 0,8) δ. There can be several centers of pitting on the pipe surface. It is experimentally found that pits interact when the distance between them doesn't exceed 2,5 mm. In this case total length is defined as the sum of lengths of individual pits. Otherwise, calculation is carried out separately for each pit.

Cited by 1 works. doi:10.17122/ntj-oil-2016-4-126-136

Authors