Creep crack growth life of high temperature pressure equipments was assessed for various crack locations and for various material properties. Surface cracks at the inner and outer surface of the vessel in the axial and circumferential directions were considered. The crak was located in the weld metal, in the parent metal or at the weld interface. Results showed that the crack at the weld interface was the most dangerous one. The crack located outside is weaker than that located inside. Safety factors of the case in which improper material properties were used due to unavailability of the correct material properties were discussed.