내화성 고강도 콘크리트 구조물의 화재 후 반발도 특성 비교

박천진, 황동규, 한창평 et al. · 한국구조물진단유지관리공학회 학술발표회 논문집 · 2009

The purpose of the study was to analyze damage characteristics and the remaining repulsion after testing a fire of high-strength concrete structure supposing a real housing building. The results of the study were as follows. Scaling and spalling were logically taken place in a pillar not mixing polylon fiber with fireproofing characteristics. However, a pillar mixing polylon fiber had a good fireproofing performance. The internal average temperature history of the real structure approached the highest temperature (713℃ on average) in about four minutes after c mbustion, and its duration time was very short as about 20 seconds. As the results of c minuing the standnud heating curve of KS 2257-1 with the internal average temperature history of the structure, the internal average temperature of the structure was beyond the standnud heating curve within enuly fs afininutes. In temperature history characteristics of an internal pillar of the structure, when polylon fiber was not mixed, repulsion on the average generally was lower about 10 than before the fire test and difference in the remaining internal force between the upper inut and the lower inut was about 5 on the average. On the other hand, when polylon fiber was mixed, average repulsion was lower about 4 than before the fire test and deviation between the upper part and the lower part was not large.

Cited by 0 works.

Authors