포름알데히드로 세리신 정착 후 정련에 의한 실크 생사의 반숙 정련
Park Geon Yong, 박창혁, Hwajin Jung et al. · 2012
To obtain the half-degummed silk yarns of 5~10% degumming losses, raw silk yarns were degummed with alkaline detergent after fixing sericin with formaldehyde. Adding above 5 g/l acetic acid or tartaric acid in 1% and 5% formaldehyde fixing baths created a lot of sericin loss during degumming with 3 g/l alkaline detergent and 2 g/l sodium carbonate after fixing sericin due to alkaline hydrolysis of sericin cross-linkage. When sericin was degummed with 3 g/l alkaline detergent after fixing with 0.1% formaldehyde at 40℃ or 60℃ for 15 min, the degumming temperature necessary to obtain satisfactory half-degumming was 70~80℃. Also, fixing sericin at 60℃ resulted in stronger sericin fixation than fixing at 40℃. However, the softener of cationic surfactant added in sericin fixing baths did not prevent the attachment of degummed silk yarns. Approximately 6.5% degumming loss was obtained when sericin was degummed at 85℃ for 30 min with 3 g/l alkaline detergent after fixing with 0.1% formaldehyde at 80℃ for 15 min and 30 min, and in case of adding 2 g/l acetic acid in fixing baths the half-degummed silk yarns of about 10% degumming losses, which were severely attached to each other, were obtained.
Cited by 0 works.