W3172496398
Koichi UESAKI, Takashi Kawakami, 英夫 武知 · Journal of Japan Institute of Light Metals · 1982
Stress corrosion cracking in welds of cold rolled Al-Zn-Mg alloy was studied by means of measurements of mechanical properties and electron microscopy. Fracture of the welded specimens in tensile testing occurs at the area 6 to 7 mm apart from fusion boundaries. SCC fracture of them, on the other hand, occurs at the HAZ about 1 mm far from the fusion boundaries independently of applied stresses, where η precipitates are formed along subgrain boundaries or grain boundaries. Preferential dissolution of these precipitates is associated strongly with initiation and propagation of SCC.
Cited by 0 works. doi:10.2464/jilm.32.229 Open-access PDF