염화물이 함유된 동결수의 동결융해 작용에 따른 콘크리트의 내동해성 및 표면 스케일링 평가에 관한 연구
노경민, 조봉석, 김영덕 et al. · 대한건축학회지회연합회 학술발표대회논문집 · 2006
combined effects of chemical actions by containing chlorides and the freeze-thaw action is also a problem which has not yet been fundamentally solved. Furthermore, surface deterioration of concrete was considered as accelerate factor of concrete durability tended to decrease. This study presents the experimental results of frost durability including resistance to freezing-thawing and suface scaling of concrete. Mixing design was proportioned with the various water-binder ratio between 0.37 and 0.47 and three different binder compositions corresponding to Type Ⅰ cement without any supplementary cementitious materials(OPC), Type Ⅱ cement with 50% blast-furnace slag replacement(BFS50), and ternary cement with Type Ⅲ cement, 15% fly sah, and 35% BFS replacement (BFS 35%+FA 15%). Test results showed that the mixing design with BFS 50% and BFS 35%+FA 15% exhibited higher durability factor than that made with OPC only. Finally, the use of blend cement containing salg can be used effectively in terms of frost durability of the concrete exposed to severe condition like as coastal environment.
Cited by 0 works.