베릴륨 불포함 치과 주조용 니켈-크롬 합금 중 금속의치상용 합금과 금속소부도재관용 합금의 부식에 관한연구
Hongsik Kim, 박수철, 송재상 · 2012
Purpose: This study examined the corrosion level by alloy type and pH, and used the corrosion levels as the dental health data. The study utilized one Ni-Cr alloy for the full and removable partial denture metal frameworks and two Ni-Cr alloys for porcelain-fused-to-metal crown, among the non-beryllium dental casting non-precious Ni-Cr alloys. Methods: The alloy specimens were manufactured in 10 and stored in the corrosive solution(pH 2.2-4.4) in the electrical water bath(37 ) for seven days. Afterwards, the metal ions were quantitatively analyzed using the ICP. Results: Of the three metal alloys, Bellabond-Plus alloy and SOLIBOND N alloy, with 22% or higher chrome chemical contents, had higher corrosion resistance than Jdium-100 alloy with 20% chrome chemical content. In all three alloys, the corrosion of Ni was highest, and metal ion corrosion was higher in the pH 2.2 corrosive solution. Conclusion: Although Ni-Cr alloy was not very corrosive, a Ni-allergic patient should not have Ni-Cr alloy prosthesis. The Ni-Cr alloy for porcelain-fused-to-metal crown should be designed for the dental porcelain to cover the whole crown.
Cited by 0 works.