산업 부산물을 이용한 칼슘설포알루미네이트의 합성

문정호, 이범재, 노재성 · 1998

Calcium sulfoaluminate, C₄A₃, was prepared for reutilizing industrial by-products, such as II-CaSO₄, Al(OH), CaF₂ and cement sludge wastes. Mixed powder was fired at 1,150℃. C₄A₃ clinkers fired at 1,150℃ were analyzed by SEM and XRD. Also were added in cement paste and mortar and characterized as setting time, flow values and compressive strength. C₄A₃ could be found in the X-ray diffraction pattern. The setting time of cement pastes added clinkers fired at 1,150℃ was shorter than that of ordinary portland cement. Also the compressive strengths of the cement mortar added clinkers was higher than those of ordinary portland cement.

Cited by 0 works.

Authors