ПОДБОР НАПОЛНИТЕЛЕЙ ДЛЯ НАРУЖНОГО ПОКРЫТИЯ НЕФТЕПРОВОДОВ
A. Ivakhnenko, А.А. Есентаева, Ю. А. Нифонтов et al. · 2021
The results of the selection of mineral filler in the development of the composition of the outer layer based on low-density polyethylene (LDPE), vegetable and mineral fillers and technical gossypol (TG) are presented. It is shown that the stability of the obtained composites is the result of increasing the degree of cross linking of the stabilized LDPE in the presence of TG. The structure of gossypol molecules and its derivatives, such as multifunctional compounds, suggests that they are not only traps for radicals formed as a result of thermal and photo oxidative destruction of LDPE, but also lead to change of the supramolecular structure of the composite due to formation of bridging bonds between various macroradicals. This fact has a significant impact on the basic physical, chemical and mechanical properties of the material, which is confirmed by the study to determine the degree of crosslinking of polymer composites. Inorganic reinforcing fillers are usually stiffer than the matrix and deform less, which leads to an overall decrease in matrix deformation, especially near the particle due to the presence of the particle/matrix boundary. In order to establish the cause of the ductile-brittle transition, functional relationships were determined to describe changes in the upper yield strength, neck extension stress and tensile strength of composites with increasing taurite concentration. The developed composition of the composite coating in mass %: vegetable filler-guzapaya-25; mineral filler-taurite (shale) - 10; savilen-5; technical gossypol-3; LDPE-50-55, fully meets the standard requirements 1390-003-11928001-01 “Steel pipes with external anti-corrosion coating based on extruded polyethylene”.
Cited by 0 works.