Влияние ориентации индентора Виккерса на разрушение щелочногалоидных кристаллов при микроиндентировании

Карыев Леонид Геннадьевич, Федоров Виктор Александрович, А. Н. Глушков et al. · Tambov University Reports Series Natural and Technical Sciences · 2000

It is discovered experimentally that micro-indentation with the Vickers pyramid of the cleavage surface of LiF single crystals causes cracking of the sample (each indentation act being always accompanied by the appearance of cracks in the {110} planes). It does not depend on the value of the load applied to the indentor when the diagonal of the imprint is oriented along the directions. The dislocation structure of the indented area of the sample, the concentration of impukituies and point defects and the temperature of the sample render influence on the degree of surface cracking.