Commercial Al-Zn-Mg alloys T6 treated and welded were tested in 5.0%NaCl +0.3%H2O2 aqueous solution. The welded alloy fractures in tensile testing at weld metals and does in SCC testing in the heat affected zone. SCC fracture occurs at a greater distance from the fusion boundary, in a shorter time and in the more typical intergranular manner, as the postweld time is prolonged. The microstructural change in accordance with postweld aging has a significant effect on SCC. Anodic dissolution of grain boundary precipitates plays an important role in SCC.