Восстановление оксидных соединений тантала парами кальция
М. В. Крыжанов, Орлов Вениамин Моисеевич · Неорганические материалы · 2023
Calcium vapor reduction of Ta2O5 and Mg4Ta2O9 has been studied at temperatures from 750 to 850°C. We have found out specific features of the pore structure of the calciothermic tantalum powders and assessed the effect of precursor particle size on the degree of reduction. To reduce the Mg4Ta2O9 tantalate with an average particle size of 2 μm, holding at a temperature of 800°C for at least 4 h was needed. Reducing the average particle size to 0.15 μm allowed us to reach complete reduction at a temperature of 750°C in just 1 h.
Cited by 1 works. doi:10.31857/s0002337x23050123 Open-access PDF
Authors
References
- Reporting physisorption data for gas/solid systems with special reference to the determination of surface area and porosity (Recommendations 1984)
- Tantalum and niobium powder preparation from their oxides by calciothermic reduction in the molten CaCl2
- The role of the reaction medium in the self propagating high temperature synthesis of nanosized tantalum powder
- Kinetics of nanoscale structure development during Mg-vapour reduction of tantalum oxide
- Making of tantalum powder using the hunter process
- Formation of broccoli-like morphology of tantalum powder
- Dielectric properties of tantalum powder with broccoli-like morphology
- CHEMICAL AND PHYSICAL PROPERTIES OF TANTALUM POWDER
- Tantalum network nanoparticles from a Ta2O5+kMg system by liquid magnesium controlled combustion
- Tantalum Powder Preparation from Ta2O5 by Calciothermic Reduction