РОЗРОБЛЕННЯ МАТЕМАТИЧНОЇ МОДЕЛІ МІЦНОСТІ ЗРОЩЕНИХ ЗАГОТОВОК ІЗ ВЖИВАНОЇ ДЕРЕВИНИ ЯЛИЦІ
L.E. Lesiv, S.V. Gayda, L. V. Salapak · Forestry Forest Paper and Woodworking Industry · 2024
The expediency of using dimensionally suitable block elements of post-consumer wood for obtaining spliced blanks for the manufacture of wood products is substantiated. Spliced blanks from used fir wood were prepared by implementing the B-plan of the second order, where the variables were the width of dimensionally suitable bars and the length of the toothed spikes in the bars. The limit of strength during static bending for spliced blanks from post-consumer fir wood was determined experimentally and an adequate mathematical (regression) model was built depending on the width of dimensionally suitable fir bars B (x1) and the length of tooth-shaped spikes in bars D (x2). It was determined that the width of the fir bar B(x1) in the construction of the jointed blanks leads to a significant increase in the strength limit during static bending σu (from 16.17 to 19.40%). On the other hand, the trend regarding the dependence of the length of toothed spikes in bars D (x2) on the increase in strength limit during static bending σu is less significant (from 10.58 to 14.03%). It was found that an increase in the length of the toothed spike from 10 to 20 mm leads to an increase in the strength limit under static bending by 5.78%, and from 10 to 30 mm – by 10.58%. It was established that the obtained strength limits σu for all samples of experimental samples of spliced blanks from post-consumer fir wood, regardless of their design, meet the regulatory requirements for primary fir wood (84.5 MPa). Based on the results of experimental studies, it was established that the maximum value of the strength limit during static bending σu = 72.2478 MPa, taken as an absolute value, can be obtained by fixing the dimensional parameters of the width of dimensionally suitable fir bars B = 56 mm and the length of the teeth – those spikes in bars D = 30 mm. Based on practical experience, it is recommended to use used wood for the production of jointed blanks with a cross-section of dimensionally suitable bars in the thickness-width ratio of no more than 1:3 with a toothed spike length of 30 mm for lattice furniture blanks, and for furniture panels and joinery boards – 10 mm.
Cited by 24 works. doi:10.36930/42245002 Open-access PDF
Authors
References
- The Circular Economy: An Interdisciplinary Exploration of the Concept and Application in a Global Context
- A investigation and analysis of characteristics of solid furniture boards made of post-consumer wood
- Determining the regime parameters for the surface cleaning of post-consumer wood by a needle milling tool
- THE INVESTIGATION OF PROPERTIES OF BLOCKBOARDS MADE OF POST-CONSUMER WOOD
- Sustainable forest biomass: a review of current residue harvesting guidelines
- MDF-FACADE TECHNOLOGIES
- A investigation of technological processes of making beds of double different designs
- Властивості вживаної деревини як важливий чинник якості конструкційних матеріалів
- Формостійкість як критерій якості столярних плит із вживаної деревини
- Comparative studies of the macro- and microstructures of stump-root wood and stemwood