Разработка морозостойких уплотнительных колец для обеспечения противопожарной безопасности в Арктических регионах РФ
Игорь Сергеевич Макаров, Afanasy A. Dyakonov, Nadezhda Nikolaevna Lazareva et al. · Pozharovzryvobezopasnost/Fire and Explosion Safety · 2025
Introduction. In the context of active Arctic development, ensuring fire safety has become a strategic task. Currently, there is a problem of hardening and breaking of sealing rings when the temperature drops to –40 °C, despite the declared operating temperature of –60 °C, according to the UHL-1 climate category. This can lead to difficulties and emergency situations during firefighting. Therefore, the development of frost-resistant sealing rings is a pressing issue. To extend their service life and improve aging resistance, it is necessary to incorporate anti-aging agents into the rubber compound formulation. The aim of the research is to identify a suitable anti-aging agent for the formulation of frost-resistant sealing rings made from SKD-V butadienе rubber, designed for use in fire hoses and hydrants. Objectives: 1. Determination of the effect of anti-aging agents on the properties of rubber compounds based on SKD-V butadienе rubber. 2. Investigation of the physico-mechanical and structural properties of elastomers. 3. Testing of the manufactured sealing rings based on the developed formulation under real operating conditions at the Ministry of Emergency Situations of the Republic of Sakha (Yakutia) and JSC “Vodokanal”. Objects and methods of research. The study examined the elastic-strength properties, wear resistance, water resistance of the specimens, hardness, residual compressive deformation, thermal aging resistance and structural properties. Results and their discussion. Antioxidants improved the elastic-strength properties, presumably due to the stabilization of the polymer network. However, when using IPPD, leaching and water discoloration were observed. Thermal aging reduced the elasticity of the specimens by 32–56 %, while combined systems demonstrated lower degradation, confirming their effectiveness. Laboratory and field tests verified the performance of the developed sealing rings in Arctic conditions in accordance with the UHL-1 climate category. Conclusions. A frost-resistan.rubber compound was developed in the course of the study. A combination of anti-aging agents, Naftam-2 and Acetonanil, was selected.
Cited by 0 works. doi:10.22227/0869-7493.2025.34.03.40-49 Open-access PDF
Authors
References
- Recent progress in the rubber antioxidants: A review
- PECULIARITIES OF EXTINGUISHING LARGE-SCALE FIRES ON THE TERRITORY OF THE RUSSIAN FEDERATION UNDER THE EXTERNAL EFFECT OF HAZARDOUS NATURAL PHENOMENA
- Carbon black distribution in natural rubber/butadiene rubber blend composites: Distribution driven by morphology
- Effect of zinc oxide/layered double hydroxide on the mechanics of silicone rubber at low temperature
- Preparation and Improved Physical Characteristics of Propylene Oxide Rubber Composites
- Cold‐Resistant Rubbers Based on Flexible Polymer Chains
- Problems Of Operation Of Elastomer Materials In The Arctic Region
- Investigation of the Plasticizer Content Effects on the Operability of the Epichlorohydrin Rubber Based Elastomeric Material during Full-Scale Test under Cold Climate Conditions and Hydrocarbon Medium Influence
- LOW TEMPERATURE SEALING BEHAVIOR EVALUATION OF ELASTOMERS IN AIRCRAFT HYDRAULIC SYSTEMS
- Production and Investigation of the Properties of Elastomers Modified with Ultradispersed (Nano) Particles