ЕКСПЕРИМЕНТАЛЬНІ ДОСЛІДЖЕННЯ ОДЕРЖАННЯ ФУНКЦІОНАЛЬНО ОРІЄНТОВАНИХ ПОРОШКІВ СИНТЕТИЧНОГО АЛМАЗУ

Н. І. Олійник, Г.Д. Ільницька, Г.А. Петасюк et al. · Наукові нотатки · 2025

Experimental studies of synthetic diamond powder of the AC20 grade with a grain size of 100/80 have shown that theinfluence of the methods of modifying the original powder (modification by high-voltage electric discharges or liquid-phaseoxidation) is reflected in the change in the adsorption-structural and morphometric characteristics of the powders: in particular,the specific surface area; specific pore volume; average pore radius; total pore volume, and the distribution of pore volume bytheir sizes. The specific surface area of the original samples tends to decrease after the modification of the powders. The studiedsamples have a developed mesoporous surface structure. The studied modification methods do not show a significant effect onthe morphometric characteristics of the powders. Comparative analysis of the results by the coefficients of linear approximationof the pore size distribution curves allows us to obtain at the quantitative level the indicator (а2/а1) of the change in the state ofthe powder surface, which can serve as a characteristic of the quality of the powder surface when studying the defectivity of thesurface of synthetic diamond grains and its influence on the operational characteristics of the diamond tool. The results obtainedprovide a basis for further development of a database for the formation of optimal indicators of the adsorption-structuralcharacteristics of synthetic diamond powders of wide functional purpose.

Cited by 0 works. doi:10.36910/775.24153966.2025.83.17

Authors