Влияние наполнителей и каталитических добавок на термоокислительную деструкцию силиконовых резин
Костылева Елена Игоревна, Копылов Виктор Михайлович, Ковязин Владимир Александрович · Известия Тульского государственного университета. Естественные науки · 2014
In work on the basis of silicon rubber and various types of fillers, for the manufacture of ceramifying insulation. Revealed that most of the fillers discussed interest micronized calcium silicate, which provides similar results for the formation of the polymer flow ash as a gradual rise in temperature, and the combustion conditions. To improve the thermal stability of interest chromium, cerium, zirconium compounds. Rubber containing proposed modifiers are starting temperature degradation 380-400 °C.