Экспериментальная оценка возможности доокисления оксидов марганцевой руды до пиролюзита
Якушевич Николай Филиппович, I. M. Kashlev, A. A. Provodova et al. · Вестник Сибирского государственного индустриального университета · 2013
Studied is the possibility of final oxidation of lower oxides of manganese contained in manganese ore to manganese dioxide. Manganese ore fractions 1 – 3 mm, containing 35 % of Mn in form cryptomelane, were oxidized in air stream and oxygen at temperature of 600 K for 2 hours. XRD analysis showed that in this oxidation mode degradation of cryptomelane lattice and manganese dioxide formation did not occur. Fig.1.
Cited by 0 works.