W589928638
Hisashi SUZUKI, 吾朗 伊藤, 克己 小山 · Journal of Japan Institute of Light Metals · 1984
The Al-4mass%Cu-(04.5)mass%Cr alloys were prepared by chill-casting, and their heat-resisting properties were examined. The amount of solute Cr quenched in Al-4%Cu alloy was about 1.5% at maximum. Resistance to over-aging was markedly increased with increasing amount of solute Cr, when the alloys were subjected to usual heat-treatments: that is, homogenization at 793K after chill-casting, water-quenching, aging at 473K and subsequent over-aging at 623K. This phenomenon would mainly be attributed to the fact that θ' formed during pre-aging became very stable both in the amount and the size, as the amount of solute Cr increased. The chill-cast Al-4%Cu-2%Cr alloy was thought to be superior to commercial heat-resisting 2219 alloy. The over-aged structures of Cr contained alloys were in detail discussed, in comparison with those of Mn contained alloys.
Cited by 1 works. doi:10.2464/jilm.34.395 Open-access PDF