充油丁苯橡胶/乙烯-乙酸乙烯酯共聚物/高抗冲聚苯乙烯热塑性硫化胶的结构与性能

赵洪玲, 王兆波 · 2010

The styrene-butadiene rubber (SBR)/ ethylene-vinyl acetate (EVA) /high impact polystyrene (HIPS) thermoplastic vulcanizate (TPV) was prepared by dynamic vulcanization, the mechanical properties and morphological structure of SBR/EVA/HIPS TPV were investigated, and the influence of aromatic oil on the viscoelasticity and stress relaxation were discussed. The results showed that for SBR/EVA/HIPS TPV in which resin phase the aromatic oil was filled, the Shore A hardness decreased obviously and permanent set decreased slightly. The size of SBR dispersed phase was in the range of 5-30 μm. With the increase of aromatic oil amount, the stress relaxation rate increased, the storage modulus decreased evidently. Compared with aromatic oil unfilled SBR/EVA/HIPS TPV, loss modulus increased remarkably and loss factor increased continuously. With the increase of frequency, the storage modulus showed linear increase, loss modulus and loss factor decreased.

Cited by 0 works.