抗菌剤添加充填用グラスアイオノマーセメントに関する研究 : 圧縮強度,崩壊率,フッ素溶出性,走査型共焦点レーザー顕微鏡による観察および抗菌性

和明 庭野 · Institutional Repositories DataBase (IRDB) · 2000

The aim of this study was to reveal the properties of glass-ionomer restorative cements containing mixed antibacterial drugs related to compressive strength, disintegration, fluoride release, surface LSM images and bactericidal efficacy. Metronidazole, cefaclor and norfloxacin were mixed in the ratio of 3:1:1 in potency. Drug mixture was also mixed with GIC powders (two RM-GICs and one conventional GIC) by 0 (as control), 3, 5, 10wt%. In the preparation of specimens, each drug-cement combination was hand-mixed in accordance with the manufacturer's instructions specific for each GIC product. 1. Compressive Strength: Compressive strength was determined for specimens stored in distilled water using a universal testing machine at a cross-head speed of 0.75/min at each storage period. (24hours, 7days, 30days) 2. Disintegration: Cumulative disintegration (%) was determined at 23 hours, 7 days and 30 days respectively. 3. Fluoride Release: The amounts of fluoride released over 24 hours were determined with a fluoride ion selective electrode. Readings were taken at 24 hours, 7 days and 30 days after immersion in distilled water. 4. Bactericidal Efficacy: Specimens were placed on the BHI-blood agar plates inoculated with bacteria sampled from carious dentin, and incubated for 7 days at 37℃ in anaerobic condition. Inhibition zone was observed. Specimens stored in distilled water for 7 days were also tested. 5. LSM Observation: Specimens were prepared using wet 1200 grid abrasive paper, and observed identically at 1500-fold magnification immediately and after 30 day-immersion in distilled water. Results 1. The more amount of mixed drugs contained in cements, the greater inhibition zone on BHI blood agar was observed. However, this also resulted in decreased mechanical and physical properties of cements. 2. Increased fluoride release from mixed drug containing GIC was thought to be related mainly to disintegration of cement matrix. 3. GIC-containing mixed drug should be applied with careful case selection and take into consideration its mechanical and pharmacological properties.

Cited by 0 works. doi:10.11501/3187308

Authors