ПОРІВНЯЛЬНІ ДОСЛІДЖЕННЯ КОРОЗІЙНОЇ СТІЙКОСТІ ЛИСТОВИХ НЕРЖАВІЮЧИХ СТАЛЕЙ ДЛЯ ПЛАКУЮЧОГО ШАРУ БІМЕТАЛІВ
Володимир Корнієнко, Dmytro Mishchenko, Сергій Борисович Бєліков et al. · The Scientific Issues of Ternopil Volodymyr Hnatiuk National Pedagogical University Series pedagogy · 2025
Purpose. Evaluation of the influence of the chemical composition and structure on the corrosion resistance of steels of different structural classes used as a cladding layer of bimetallic reactors and other devices of titanium-magnesium production. Research methods. In order to choose a rational cladding layer of the developed bimetal, a comparative analysis of the corrosion resistance of steels 12X18Н9, 10X14AГ15 and 08X18T1 and steels 04X18ч, 03X18TБч and 03X17H3Г9МБДЮч, taken as standards for comparison, was carried out [1]. Titanium tetrachloride and a one-molar solution of sulfuric acid were used as chemically active media. Results. The results of the investigation of the corrosion resistance of steels of different structural classes by gravimetric and potentiometric methods in chemically active environments showed that the most suitable option for the cladding layer is steel 03Х17Н3Г9МБДЮч, which has similar coefficients of linear thermal expansion and high corrosion resistance to the base of bimetal - 14Х17Н13МБч [2]. Scientific novelty. It was established that the use of bimetal with a cladding layer made of 03X17H3Г9MBДЮч, 03X18Н or 04X18ч steel reduces the nickel impurity content by 10 times or more in the titanium sponge during the reduction process. Practical value. The use of a bimetal with a base steel of 14X17H13MBч in combination with a cladding layer of steel 03X17H3Г9MБДЮч makes it possible to obtain a titanium sponge that is particularly clean of nickel impurities and will significantly expand the scope of use in the aviation and rocket industry.
Cited by 0 works.