Дослідження кінетики процесу отвердження епоксидного полімеру механічними та теплофізичними методами
Тарас Січкар, Максим Олександрович Рокицький, Л. Ю. Благодаренко et al. · The Scientific Issues of Ternopil Volodymyr Hnatiuk National Pedagogical University Series pedagogy · 2025
The article investigates the kinetics of curing in epoxy polymers using a combination of ultrasonic acoustic methods and thermophysical measurements. Epoxy materials are widely used in engineering, construction, and composite technologies, and their final properties depend strongly on the structural transformations occurring during curing. Despite the broad application of epoxy systems, detailed information regarding the evolution of their physical properties during the curing process remains limited, which highlights the relevance of the study. The compositions based on the epoxy resin ED-20 cured with polyethylene polyamine (PEPA), including systems modified with dibutyl phthalate (DBF) and epoxy ether (EET) are examined. Structural changes during curing are monitored by measuring the ultrasonic wave velocity and attenuation using an echo-pulse method. This approach enables real-time observation of transitions from the initial liquid mixture to the gel state and finally to the glassy polymer. Because ultrasonic parameters are highly sensitive to changes in molecular mobility, crosslinking density, and internal structural rearrangements, they serve as effective indicators of the curing stages. The study identifies three main stages of epoxy polymer curing. The first stage, up to ap-proximately 50 minutes, corresponds to the onset of chemical interaction between the resin and hardener. During this period, heat release from exothermic reactions results in increasing temperature and decreasing thermal conductivity, reflecting lowered viscosity and enhanced molecular mobility. The second stage (≈ 50–110 minutes) marks the formation of a gel network. Both ultrasonic velocity and thermal conductivity increase significantly, indicating rapid growth of crosslink density. This interval also corresponds to the maximum exothermic effect. The final stage (≈ 250–300 minutes) represents the transition to the glassy state, where seg-mental mobility becomes greatly restricted and the curing process effectively stops, reaching about 50–60% conversion. Completion of curing is possible only at higher temperatures. In parallel, thermophysical measurements based on temperature evolution and thermal conductivity provide independent confirmation of the observed stages. A special linear probe containing a heater and thermocouple is used to measure heat propagation dynamics, enabling correlation with ultrasonic results. These data reinforce the understanding of structural trans-formations occurring throughout curing. The authors emphasize the practical significance of the findings. Determining the characteristic points of gelation and vitrification allows optimization of industrial processes involving epoxy polymers, such as extrusion, casting, and forming. Knowledge of the cure kinetics helps define the allowable residence time of the polymer in technological equipment before it becomes immobile due to vitrification. Furthermore, the experimental setup developed in the study enables repeated use of the measurement probe and retention of the cured sample for additional analysis. Overall, the research demonstrates that combined acoustic and thermophysical methods are highly effective for characterizing the kinetics and structural evolution of epoxy polymers, contributing both to fundamental understanding and applied material engineering.
Cited by 0 works. Open-access PDF