表面被覆した炭素鋼の磨耗特性

詢 相馬 · Institutional Repositories DataBase (IRDB) · 1997

In order to raise the wear resistance 。f structural carbon steel Of ]ーS S350, the surface was coated with WC by spark hardening apparatus "Penetron" and the wear test was performed by Ohkoshi's wear test machine.1) 2) 6) The results obtained were as follows.A coated layer of about 10 " m was obtainable with 1 min/cm2 and 15 " m with 2 min/cm2 easily by Penetron.The hardness of coated layer reached HV 550~600, whereas the matrix was about HV 250.The inside of coated later was a diffused hardened layer and the hardness decreased gradually and reached the matrix hardness.With the final load of 21 N, the wear amount decreased about 80 % for both coated layers compared to non-coated iron.With the final load of 31 N, the wear amount decreased remarkably for the sliding speed of 0.9 and 2.0 m/s, whereas the wear resistance varnished for 0.1 and 3.6 m/s._With the final load of 62 N, the wear amount decreased for 0.1 and 0.9 m/s, Whereas the wear resistance varnished for 2.0 and 3.6 m/s.The surface-coated carbon steel was proved to be utilized as the wear-resistant steel if the conditions of utilization are selected reasonably.

Cited by 0 works. doi:10.32150/00004709 Open-access PDF

Authors