黒鉛に打ち込まれた水素同位体の脱離機構と再結合係数

国昭 渡辺, 完 芦田 · Institutional Repositories DataBase (IRDB) · 1985

Kinetics and mechanisms were studied for the thermal release of hydrogen isotopes implanted into pyrolytic graphite. The kinetic measurements were carried out with mass analyzed thermal desorption spectroscopy. The desorption spectra consisted of three peaks, Ⅰ, Ⅱ, and Ⅲ. The peak Ⅰ obeyed the second order kinetics regarding the amount of trapped hydrogen isotope atoms. The recombination factors averaged over the sub-surface layer were determined as kr(H2)=(13.0x10-19)exp(-44.0x103/RT) [cm4/sec・molec] kr(D2)=(7.18x10-19)exp(-44.0x103/RT) kr(T2)=(5.26x10-19)exp(-44.0x103/RT) The pseudo surface recombination factors were also determined as ks K2 (H2)=(4.68x10-19)exp(-44.0x103/RT) [cm2/sec・molec] ks K2 (D2)=(2.58x10-19)exp(-44.0x103/RT) ks K2 (T2)=(1.89x10-19)exp(-44.0x103/RT) It was concluded that the rate determining step for desorption forming the peak Ⅰ was the surface recombination reaction of hydrogen isotope atoms trapped on the normal graphite lattice of the basal plane.

Cited by 0 works. doi:10.15099/00006338

Authors