金属光造形複合加工法に関する研究: 余剰硬化部の生成過程

諭 阿部, 喜万 東, 勲 不破 et al. · Institutional Repositories DataBase (IRDB) · 2007

In the Milling Combined Laser Metal Sintering Process, the sticking-out sintering part is formed in the side of the work piece when the following layer is sintered after completing the side of the work piece by milling process.The processing time is long, because the overlapped area to have contained the sticking-out part has to be milled.Therefore, making the sticking-out sintering part small is required.In this paper, it is evaluated how it is formed in the sintering process after the milling process.Width and depth of the sticking-out sintering part is fixed by the sintering in the first layer after the milling process.As the laser irradiation range sticks out outside than the edge, depth of the sticking-out sintering part becomes deep extremely.

Cited by 0 works. doi:10.24517/00050009 Open-access PDF