溶接ビードレーザスキャナで測定した溶接継手止端部の応力集中係数によるケミカルタンカーの品質管理

卓也 荒金, 尚憲 鍬, 雄介 春山 et al. · Institutional Repositories DataBase (IRDB) · 2024

In this study, the welded joint surface shapes of fatigue test specimens simulated as the cruciform welded joints between the transverse bulkhead and the double bottom were measured by a weld bead laser scanner and the stress concentration factors (KtL) of the welded joint of the specimens were calculated by using the conventional estimating equation with the measured geometrical data of the welded parts. In addition, the static FEM analysis was also conducted to obtain the stress concentration factors (KtF) using the same measured data. Comparing the stress concentration factors KtL and KtF with the stress concentration factor KtS calculated by the conventional estimating method with silicon mold, it was shown that KtL and KtF values were about the same as that of KtS. In addition, the representative value of the fatigue strength at 2×10 6 cycles for cruciform welded joint was derived considering the fatigue test results using the cruciform welded joint specimens and the results of previous studies, the allowable stress concentration factor (KtA) was presumed based on the representative value of fatigue strength and design S-N curve for cruciform welded joints. As a result, it is proposed that the guarantee which fatigue crack initiation does not occur at the toe of welded joint can be valid when the geometry of weld joints in the cargo tank structure under construction at shipbuilding site is measured by using the weld bead laser scanner and immediately the stress concentration factor KtL or KtF is calculated and the value is evaluated less than KtA. This is a revolutionary technique in terms of quality control and assurance of shipbuilding.

Cited by 0 works. Open-access PDF

Authors