感染創に使用したヘパリン湿潤コラーゲン型創傷被覆材の臨床経験
卓嗣 東山, 直樹 根岸, 玲子 東山 et al. · Institutional Repositories DataBase (IRDB) · 1992
The bacterial infected wounds(MRSA or必θπ40伽%αsα〃駕gゴ〃osσ)were covered with artificial templates composed of silastic membranes and porous atel(レcoUagens immersed with heparin solution (200U/m1). Two weeks after coverage, thin split・thickness skin(11/1000 inches)was grafted on the template after removing silastic membrane. Although infectiqn was present, the skin graft took in wound perfectly. Three months after coverage, the contraction and pigmentation of the graft were observed in the minimum grade. Histological examination was performed at 1,2,3and 4 weeks after coverage. The capillary vessels extending to the middle layer of the artificial dermis was observed and the initial pr㏄ess of vascularization was recognized in the superficial layer l week after coverage. Pseudo-dermination were also observed in good condition,2,3, and 4 weeks aftef the coverage. From those clinical result, confirmation was definitely made that heparin at its clinical usage accelerated vascularization in the dermis and then formed an immunosurfaced grouhd. It was surmised that heparin has an activity of strengthening, physiologically, the cross・董inking among the molecules to atelo・collagen. 緒 言 形成外科領域において,外傷熱傷等による皮
Cited by 0 works. Open-access PDF