正負繰り返し負荷を受ける合板釘着張り耐力壁のせん断性能
祐志 今西, Hiroshi IMANISHI, 康寿 佐々木 et al. · Institutional Repositories DataBase (IRDB) · 1997
Racking tests under the conditions of cyclic loading with constant deformation (± 1/120 rad and ± 1/300 rad) and monotonous increase of loading were conducted on plywood nailed walls. The shearing performance of the walls is discussed in relation to the cyclic deformation value and to the number of cycles. The cyclic loading fatigue tests showed that maximum values for the shearing force decreased logarithmically with increases in the number of cycles and that the decreasing ratios were larger for ± 1/120 rad cyclic deformation. The residual deformation increased untill about the 50th cycle, regardless of the cyclic deformation value, and then decreased with increases in the number of cycles. The absorbed energy, which were calculated from the shearing force-deformation curves obtained from the fatigue tests, decreased as the number of cycles increased, the decrease being especially sharp untill about the 3rd cycle. The monotonous increase loading tests after the fatigue tests showed that the shearing performance of the walls decreased with increases in the cyclic deformation value. For example, the shear load factor in case of ± 1/300 rad cyclic deformation was 1.95, and that in case of ± 1/120 rad cyclic deformation was 0.738, the former being about 2.6 times larger than the latter.
Cited by 0 works. doi:10.18999/nagufs.16.7