非水溶媒からのアルミニウムめっき薄膜の陽極酸化
未来 後藤, 宣朗 渡辺, 祐紀 久我 et al. · Institutional Repositories DataBase (IRDB) · 2013
Recently, it is possible to deposit aluminum from non-aqueous solution by using non-aqueous solvent. An anodic oxidation is very common to improve corrosion resistance and micropore formation. However there is almost no investigation about anodic oxidation of plated aluminum film. The plated aluminum films were anodized to create micropore. An oxalic acid was used to anodize Al plated film. Five conditions had been investigated to create micropores by changing oxalic acid concentration, applied voltage and treated time. The best condition was 0.1 mol/l oxalic acid concentration, 40V applied voltage and 5 minutes treatment time. In this study, the plated Al films were not uniformly formed. The area that was not uniformly formed, micropore, wave-like structure and so on, showed heterogeneous anodic oxidation. Therefore, an uniform Al film formation is necessary for micropore formation. The plated aluminum film area which showed some roughness also showed heterogeneous anodic oxidation. However, there was some regularity of micropore arrangement. The roughness was one of the most important factors to improve regularity. An mixture acidic solution of phosphoric acid, sulfuric acid and oxalic acid, whose mixing ratio was 15:4:1, was used for chemical polishing to improve flatness of plated aluminum film. The chemical polishing treatment at 60℃ for 1 minute made the plated Al film flat. After anodic oxidation with 40V for 5 minutes and with 60V for 5 minutes, micropores with uniform regularity have been obtain. Distance between micropores formed by 60V was longer than that by 40V.
Cited by 0 works. Open-access PDF