泥炭の過マンガン酸カリ及び過酸化水素酸化について

満雄 佐々木, 晴望 平野, 晴望 平野 et al. · Institutional Repositories DataBase (IRDB) · 1963

For the purpose of increasing humic acid content in peat,we carried out both content oxidation with dil. nitric acid and air oxidation. So as to obtain a product humic content of about 60 or 63%,the former process took l.5 hrs. and the latter l hr.. ln this paper,in order to compare with the above process,researches of oxidation with potassium permangate or hydrogen peroxide are dealt with. 0n oxidation,the maximum humic acid content in peat was 51%at 60℃,6 hrs.,N/5 KMn0_4,and then at 60℃,3hrs.,1%H_2O_2. As a result of this researches,the use of KMn0_4,0r H_2()_2 as oxidizing agent was unsuccessful