日本古代土器の熱的性質について(その2)

甲子郎 梅田, 甲子郎 梅田, 甲子郎 梅田 · Institutional Repositories DataBase (IRDB) · 1968

The Jomon and Yayoi potteries generally show the drying shrinkage at about 200゜C and the firing shrinkage at about 650゜C in the measurement of the thermal expansion. The firing shrinkage of the Sueki potteries takes place between 900゜C and 1000゜C. The temperature of the firing shrinkage suggests the upper limit of the temperature which were mainly kept during the burning of potteries. The Jomon and Yayoi potteries are similar in the chemical and mineralogical components and the temperature of burning. The Sueki Potteries are considerably better in the selection of raw material and higher in the temperature of burning than them.