Abstract. The use of material-extrusion polymer parts in auxiliary aircraft components is constrained by insufficient comparative data on the retention of their mechanical properties after prolonged contact with aviation fuel. The aim of the study was to quantify changes in the tensile properties of selected additively manufactured thermoplastics after immersion in technical (aviation) kerosene and to identify the materials with the highest property retention. Six commercial thermoplastics were investigated. Specimens were tested before immersion and after 7 and 30 days of kerosene exposure. Elastic modulus, 0.2% proof stress, and ultimate tensile strength were determined, and a retention coefficient was calculated for each property. After 30 days, PETg PLX retained 97.8% of its initial ultimate tensile strength and 98.8% of its proof stress. For all other materials, ultimate-strength retention did not exceed 58.8%; ABS 3DP showed the lowest values, retaining 11.8% and 7.8%, respectively. Changes in elastic modulus did not consistently correspond to the loss of strength. A quantitative ranking based on the simultaneous retention of two strength characteristics was obtained. PETg PLX was identified as the most resistant candidate for further qualification, and the combined retention of ultimate tensile strength and proof stress was established as a screening criterion for additively manufactured components exposed to aviation kerosene.

Cited by 0 works.

Authors